Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 10322B050 0.050" (1.27 mm) Fully Cured Silicone Rubber with Polyethylene Liner.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Liner: Polyethylene Material: Fully Cured Silicone RubberProduct Use: Anti-Static Vacuum BaggingAppearance: Black elastomeric sheetThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Liner
1270 microns
50.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Silicone Property; ASTM D2240
Tensile Strength 4.83 MPa
700 psi
Silicone Property; ASTM D412
Elongation at Break 290 %
290 %
Silicone Property; ASTM D412
Compression Set 25 %
25 %
Silicone Property; Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Black
Total Product Weight (oz/yd2) 44.6
Arlon SQA-TMS-025