Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 102 microns
4.00 mil
Side 1; Arlon SQA-TMS-003
102 microns
4.00 mil
Side 2; Arlon SQA-TMS-003
381 microns
15.0 mil
Substrate; Arlon SQA-TMS-003
584 microns
23.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 4.83 MPa
700 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 190 %
190 %
Silicone Property; Arlon SQA-TMS-008
Peel Strength 0.771 kN/m
4.40 pli
Bond Strength; Arlon SAQ-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
Arlon SQA-TMS-019
Electrical Properties Metric English Comments
Dielectric Strength >= 20.0 kV/mm
>= 509 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Gray
Total Product Weight (oz/yd2) 15.9
Arlon SQA-TMS-025