Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
Side 2; Arlon SQA-TMS-003
254 microns
10.0 mil
Side 1; Arlon SQA-TMS-003
356 microns
14.0 mil
Substrate; Arlon SQA-TMS-003
813 microns
32.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 5.52 MPa
800 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 500 %
500 %
Silicone Property; Arlon SQA-TMS-008
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 12.7
Arlon SQA-TMS-025