Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
127 microns
5.00 mil
PET Carrier; Arlon SQA-TMS-003
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
381 microns
15.0 mil
Side 1; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Compound Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Compound Property; ASTM D412
Elongation at Break 500 %
500 %
Compound Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
rated per UL card E54153
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 14.8
Arlon SQA-TMS-025