Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 48360X005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 48360X005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111) flame resistance requirements.Product Use: Flexible hose/duct substrateAppearance: Gray silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 38.1 microns
1.50 mil
Interleave
50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
127 microns
5.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
Silicone Property; ASTM D2240
Tensile Strength 0.689 MPa
100 psi
Silicone Property; ASTM D412
Elongation at Break 275 %
275 %
Silicone Property; ASTM D412
Peel Strength 0.578 kN/m
3.30 pli
(S1 to S2) Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 0.00
0.00
[sec], After Flame Time
0.60
0.60
[in], Flame Propagation
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
White
Substrate
Total Product Weight (oz/yd2) 5.1
Arlon SQA-TMS-025
Copyright © lookpolymers.com All Rights Reserved