Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
88.9 microns
3.50 mil
Side 1; Arlon SQA-TMS-003
88.9 microns
3.50 mil
Side 2; Arlon SQA-TMS-003
254 microns
10.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 4.83 MPa
700 psi
Silicone Property; ASTM D412
Elongation at Break 200 %
200 %
Silicone Property; ASTM D412
Peel Strength 0.894 kN/m
5.10 pli
Bond Strength (S1 to S1); ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
E54153
UL RTI, Mechanical without Impact 220 °C
428 °F
E54153
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
1.50 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.0250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 9.5
Arlon SQA-TMS-025