Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 48B10R005 0.005" (0.127 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInformation provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 50.8 microns
2.00 mil
Side 1; Arlon SQA-TMS-003
63.5 microns
2.50 mil
Interleave
76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
127 microns
5.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 6.72 MPa
975 psi
Silicone Property; ASTM D412
Elongation at Break 275 %
275 %
Silicone Property; ASTM D412
Tear Strength 9.64 kN/m
55.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 0.701 kN/m
4.00 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test >= 1.0
>= 1.0
[sec], Flame and Glow; FAR 25.853 App.F, P.1,.Aii
>= 1.0
>= 1.0
[in], Char Length; FAR 25.853 App.F, P.1,.Aii
Electrical Properties Metric English Comments
Dielectric Strength 35.4 kV/mm
900 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 149 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 300 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Red
Substrate
Total Product Weight (oz/yd2) 4.8
Arlon SQA-TMS-025
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved