Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
114 microns
4.50 mil
Side 1; Arlon SQA-TMS-003
140 microns
5.50 mil
Substrate; Arlon SQA-TMS-003
254 microns
10.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property; ASTM D2240
Tensile Strength 5.52 MPa
800 psi
Silicone Property; ASTM D412
Elongation at Break 225 %
225 %
Silicone Property; ASTM D412
Tear Strength 15.8 kN/m
90.0 pli
Die B, Silicone Property; ASTM D624
Peel Strength 1.23 kN/m
7.00 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 26.6 kV/mm
675 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 10.3
Arlon SQA-TMS-025