Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 510-638R-50 0.008" (0.203 mm) Silicone Rubber Coated Fiberglass

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 510-638R-50 0.008" (0.203 mm) Silicone Rubber Coated Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
48 inches overall usable width. Design/Construction: Fiberglass fabric primed for adhesion to silicone elastomers vulcanized with organic peroxides.Style: 7628Weave: Plain Count (ends x picks): 44 x 32Appearance: Red silicone rubber of woven fiberglass fabricThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.9 °C
60.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Recommended Application Pressure 0 - 5 Mpa
Service Life (225°C and 2.07MPa)
Total Product Weight (oz/yd2) 6
Arlon SQA-TMS-025
Uncoated Fabric Break Strength 200 lb/in
Arlon SQA-TMS-026, Fill Direction
275 lb/in
Arlon SQA-TMS-026, Warp Direction
Copyright © lookpolymers.com All Rights Reserved