Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave 1
76.2 microns
3.00 mil
Interleave 2
152 microns
6.00 mil
Side 1; Arlon SQA-TMS-003
152 microns
6.00 mil
Side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Silicone Property; ASTM D2240
Tensile Strength 7.329 MPa
1063 psi
Silicone Property; ASTM D412
Elongation at Break 134 %
134 %
Silicone Property; ASTM D412
Tear Strength 25.2 kN/m
144 pli
[ppiw], Die B, Silicone Property; ASTM D624
Peel Strength 0.526 kN/m
3.00 pli
[ppiw], Bond Strength to 6061 aluminum (90° peel test); Arlon-SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Red
Substrate
Total Product Weight (oz/yd2) 21.6
Arlon SQA-TMS-025
Users viewing this material also viewed the following: