Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51588R019 0.019" (0.483 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2, Layer 1: Cured Silicone RubberSide 2, Layer 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Side 1, Silicone Property; Arlon SQA-TMS-024
1.34 g/cc
0.0484 lb/in³
Side 2, Layer 2, Silicone Property; Arlon SQA-TMS-024
1.56 g/cc
0.0564 lb/in³
Side 2, Layer 1, Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
88.9 microns
3.50 mil
Side 1; Arlon SQA-TMS-003
88.9 microns
3.50 mil
Side 2, Layer 2; Arlon SQA-TMS-003
102 microns
4.00 mil
Side 2, Layer 1; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
483 microns
19.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 37
37
Side 1, Silicone Property; ASTM D2240
37
37
Side 2, Layer 2, Silicone Property; ASTM D2240
55
55
Side 2, Layer 1, Silicone Property; ASTM D2240
Tensile Strength 3.65 MPa
530 psi
Side 2, Layer 1, Silicone Property; ASTM D412
6.55 MPa
950 psi
Side 1, Silicone Property; ASTM D412
6.55 MPa
950 psi
Side 2, Layer 2, Silicone Property; ASTM D412
Elongation at Break 300 %
300 %
Side 2, Layer 1, Silicone Property; ASTM D412
620 %
620 %
Side 1, Silicone Property; ASTM D412
620 %
620 %
Side 2, Layer 2, Silicone Property; ASTM D412
Tear Strength 7.01 kN/m
40.0 pli
Side 2, Layer 1, Silicone Property; ASTM D624
26.3 kN/m
150 pli
Side 1, Silicone Property; ASTM D624
26.3 kN/m
150 pli
Side 2, Layer 2, Silicone Property; ASTM D624
Peel Strength 1.40 kN/m
8.00 pli
Bond Strength; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB

@Temperature 200 °C
HB

@Temperature 392 °F
per card E54153
Electrical Properties Metric English Comments
Dielectric Strength 28.7 kV/mm
728 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 21.7
Arlon SQA-TMS-025