Arlon 51943C014 0.014" (0.356 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 51943C014 0.014" (0.356 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness >= 76.2 microns
>= 3.00 mil
Side 1
>= 76.2 microns
>= 3.00 mil
Side 2
76.2 microns
3.00 mil
Polyethylene, Interleave
203 microns
8.00 mil
Prime Coated 7628 Fiberglass, Substrate
318 - 394 microns
12.5 - 15.5 mil
Overall
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Compound Property
Tensile Strength 7.24 - 8.62 MPa
1050 - 1250 psi
Compound Property
Elongation at Break 450 - 550 %
450 - 550 %
Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
per card E54153
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 23.9 °C
12.0 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Brown
Total Product Weight (oz/yd2) 13.8 - 16.8
Uncoated Fabric Break Strength 200 lb/in
Fill Direction, Substrate Property
250 lb/in
Warp Direction, Substrate Property