Material Notes:
Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 88.9 microns
3.50 mil
side 1; Arlon SQA-TMS-003
140 microns
5.50 mil
side 2; Arlon SQA-TMS-003
203 microns
8.00 mil
substrate; Arlon SQA-TMS-003
432 microns
17.0 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
silicone property; ASTM D2240
Tensile Strength, Ultimate 8.89 MPa
1290 psi
silicone property; ASTM D412
Elongation at Break 150 %
150 %
silicone property; ASTM D412
Adhesive Bond Strength 0.0207 MPa
3.00 psi
Arlon SQA-TMS-011
Tear Strength 14.5 kN/m
83.0 pli
Die B; silicone property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-1
V-1
Electrical Properties Metric English Comments
Dielectric Strength 31.9 kV/mm
811 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 23.9 °C
6.00 Month

@Temperature 75.0 °F
Descriptive Properties Value Comments
Color Gray