Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 406 microns
16.0 mil
Substrate; Arlon SQA-TMS-003
584 microns
23.0 mil
Side 1; Arlon SQA-TMS-003
584 microns
23.0 mil
Side 2; Arlon SQA-TMS-003
1570 microns
62.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
Silicone Property; Arlon SQA-TMS-014
81
81
Product Property; Arlon SQA-TMS-014
Tensile Strength 8.62 MPa
1250 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 240 %
240 %
Silicone Property; Arlon SQA-TMS-008
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 - 300 °C

@Pressure 0.000 - 10.0 MPa
302 - 572 °F

@Pressure 0.000 - 1450 psi
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 22.8 °C
60.0 Month

@Temperature 73.0 °F
Descriptive Properties Value Comments
Color Red
Service Life 80 hours
at 225°C and 6.9 MPa
Total Product Weight (oz/yd2) 65.6