Arlon 920-10Bxx-P0 0.020" Self-Fusing Silicone Rubber Tape

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 920-10Bxx-P0 0.020" Self-Fusing Silicone Rubber Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
1 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Design/Construction:Interleave: 2.5 mil PolyethyleneRubber: Cured Self-fusing Silicone RubberCross-section: RectangularThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 508 microns
20.0 mil
Overall Rubber Thickness; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 11.40 MPa
1653 psi
Silicone Property; Arlon SQA-TMS-009
Elongation at Break 519 %
519 %
Silicone Property; Arlon SQA-TMS-009
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 260 °C
500 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Allis Chalmers Tack (inches) 0.125
Arlon SQA-TMS-013
Color Black