Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon A4020-C004FR 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate  .pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 15% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film FAR 25.853 Recognition: Product is designed to meet the FAR 25.853 App. F, P.1,.Aii flame resistance requirements but is not recognized by an FAA test Laboratory. UL94V-0: The product is designed to meet UL94V-0 flame resistance requirements but is not recognized by Underwriters Laboratories. This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Interleave
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
508 microns
20.0 mil
Overall; Arlon SQA-TMS-003
25400 microns
1000 mil
Width; Arlon SQA-TMS-012
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Silicone Property; ASTM D2240
Tensile Strength 7.03 MPa
1020 psi
Silicone Property; ASTM D412
19.7 MPa
2850 psi
Product Property; Arlon SQA-TMS-048
Elongation at Break 30 %
30 %
Tape Property; Arlon SQA-TMS-048
450 %
450 %
Silicone Property; ASTM D412
Peel Strength 1.58 kN/m
9.00 pli
Adhesion Strength, Tape Property; Arlon SQA-TMS-047
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 27.6 kV/mm
700 kV/in
Tape Property; ASTM D149
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Brown
White
Substrate