Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Used in the RF and microwave industries.Information provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.84 g/cc
0.103 lb/in³
Water Absorption 0.080 %
0.080 %
Outgassing - Total Mass Loss 0.00 %
0.00 %
Collected Volatile
0.020 %
0.020 %
Total Mass Loss
Mechanical Properties Metric English Comments
Peel Strength 0.877 kN/m
5.00 pli
Thermal Properties Metric English Comments
CTE, linear 14.0 µm/m-°C
7.78 µin/in-°F
x direction
16.0 µm/m-°C
8.89 µin/in-°F
y direction
CTE, linear, Transverse to Flow 37.0 µm/m-°C
20.6 µin/in-°F
z direction
Thermal Conductivity 0.645 W/m-K
4.48 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 10

@Frequency 1.00e+10 Hz
10

@Frequency 1.00e+10 Hz
9.7

@Thickness 0.610 mm
9.7

@Thickness 0.0240 in
9.8

@Thickness 2.36 mm
9.8

@Thickness 0.0930 in
Dissipation Factor 0.0030

@Frequency 1.00e+10 Hz
0.0030

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -233