Material Notes:
This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Silicone Property; Arlon SQA-TMS-024
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
Silicone Property; ASTM D2240
Tensile Strength 8.584 MPa
1245 psi
Silicone Property; ASTM D412
Elongation at Break 565 %
565 %
Silicone Property; ASTM D412
Tear Strength 17.5 kN/m
100 pli
Silicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red