Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R35782R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R35782R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 FiberglassThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Laminated Metalized Polymer Film; Arlon SQA-TMS-003
38.1 microns
1.50 mil
Side 1; Arlon SQA-TMS-003
203 microns
8.00 mil
Substrate; Arlon SQA-TMS-003
267 microns
10.5 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Silicone Property; ASTM D412
Elongation at Break 400 %
400 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Shrinkage 0.50 %

@Temperature 230 °C,
Time 1800 sec
0.50 %

@Temperature 446 °F,
Time 0.500 hour
Metalized Polymer Film Property
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature 21.1 °C
12.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Total Product Weight (oz/yd2) 11