Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon R36029R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R36029R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Silicone Property, Layer 1; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Silicone Property, Layer 2; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Interleave
102 microns
4.00 mil
Layer 1; Arlon SQA-TMS-003
152 microns
6.00 mil
Layer 2; Arlon SQA-TMS-003
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
711 microns
28.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Silicone Property, Layer 1; ASTM D2240
60
60
Silicone Property, Layer 2; ASTM D2240
Tensile Strength 4.83 MPa
700 psi
Silicone Property, Layer 1; ASTM D412
4.83 MPa
700 psi
Silicone Property, Layer 2; ASTM D412
Elongation at Break 200 %
200 %
Silicone Property, Layer 1; ASTM D412
200 %
200 %
Silicone Property, Layer 2; ASTM D412
Peel Strength 1.58 kN/m
9.00 pli
Bond Strength (S1 to S1); ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 19.7 kV/mm
500 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 135 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 275 °F
Recommended Cure Cycle
Shelf Life 3.00 Month

@Temperature 23.9 °C
3.00 Month

@Temperature 75.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 26.7