Arlon R37503G015 0.015" (0.381 mm) Cured Fluorosilicone Rubber

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon R37503G015 0.015" (0.381 mm) Cured Fluorosilicone Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneSide 2: Cured Fluorosilicone RubberSubstrate: Polyester FabricSide 2: Cured Fluorosilicone Rubber Substrate Weave: PlainFabric Count (Wrap x Fill): 88 x 80Appearance: Green silicone gum and on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
Fluorosilicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Interleave
127 microns
5.00 mil
Side 1; Arlon SQA-TMS-003
127 microns
5.00 mil
Side 2; Arlon SQA-TMS-003
127 microns
5.00 mil
Substrate; Arlon SQA-TMS-003
381 microns
15.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
Fluorosilicone Property; ASTM D2240
Tensile Strength 7.10 MPa
1030 psi
Fluorosilicone Property; ASTM D412
Elongation at Break 410 %
410 %
Fluorosilicone Property; ASTM D412
Tear Strength 19.1 kN/m
109 pli
Die B, Fluorosilicone Property; ASTM D624
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Green
Fuel Resistance 17.5
Fuel A Resistance, Product Property, ASTM D471
23.2
Fuel C Resistance, Fluorosilicone Property, ASTM D471
26.6
Fuel C Resistance, Product Property, ASTM D471
8.1
Fuel CM85 Resistance, Fluorosilicone Property, ASTM D471
8.9
Fuel CM85 Resistance, Product Property, ASTM D471
9.6
Fuel A Resistance, Fluorosilicone Property, ASTM D471
Mullen Burst Strength 213
ASTM D751
Plasticity 2.3 mm
Arlon SQA-TMS-005
3.21 mm
Arlon SQA-TMS-005
Uncoated Fabric Break Strength 109 ppiw
Fill Strength, ASTM D751
155 ppiw
Warp Strength, ASTM D751