Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cured Silicone RubberLiner: Polyethylene This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 63.5 microns
2.50 mil
Side 1; Arlon SQA-TMS-003
63.5 microns
2.50 mil
Side 2; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Substrate; Arlon SQA-TMS-003
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 77
77
Silicone Property; ASTM D2240
Tensile Strength 4.72 MPa
685 psi
Silicone Property; ASTM D412
Tensile Strength, Yield 24.5 MPa

@Strain <=1.00 %
3550 psi

@Strain <=1.00 %
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 120 %
120 %
Silicone Property; ASTM D412
Poissons Ratio 0.50
0.50
Approximately, Silicone Property
Thermal Properties Metric English Comments
CTE, linear 150 µm/m-°C

@Temperature 20.0 - 160 °C
83.3 µin/in-°F

@Temperature 68.0 - 320 °F
Silicone Property; ASTM E 831
Specific Heat Capacity 0.820 J/g-°C

@Temperature 100 °C
0.196 BTU/lb-°F

@Temperature 212 °F
Silicone Property; Arlon SQA-TMS-052
Thermal Conductivity 1.40 W/m-K

@Temperature 100 °C
9.72 BTU-in/hr-ft²-°F

@Temperature 212 °F
Silicone Property; ASTM E 1530
1.70 W/m-K

@Pressure 30.0 MPa,
Temperature 50.0 °C
11.8 BTU-in/hr-ft²-°F

@Pressure 4350 psi,
Temperature 122 °F
Product Property; Arlon SQA-TMS-054
Maximum Service Temperature, Air 95.6 °C
204 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg 118 °C
244 °F
Silicone Property; ASTM D3418
Electrical Properties Metric English Comments
Dielectric Constant 6.91

@Frequency 1.00e+6 Hz
6.91

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
Dielectric Strength 25.2 kV/mm
640 kV/in
ASTM D149
Dissipation Factor 0.0044

@Frequency 1.00e+6 Hz
0.0044

@Frequency 1.00e+6 Hz
Silicon Property; IPC TM 650 - 2.5.5.3
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.0 - 27.0 °C
60.0 Month

@Temperature 69.8 - 80.6 °F
From date of manufacture
Descriptive Properties Value Comments
Color Gray
Naturally White
Substrate
Plasticity 2.3 mm
Arlon-SQA-TMS-005
Total Product Weight (g/m2) 432
Arlon SQA-TMS-025