Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Thermabond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260 or Lord Chemical Chemlock® 607Product Use: Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Appearance: White, High viscosity gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 25.4 microns
1.00 mil
Liner
76.2 microns
3.00 mil
Carrier
203 microns
8.00 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Silicone Property; ASTM D2240
Tensile Strength 4.48 MPa
650 psi
Silicone Property; ASTM D412
Elongation at Break 25 %
25 %
Silicone Property; ASTM D412
Shear Modulus 0.0000689 GPa
0.0100 ksi
ASTM D1002
Shear Strength 2.62 MPa
380 psi
Lap Shear Strength; ASTM D1002
Thermal Properties Metric English Comments
Thermal Conductivity 0.800 W/m-K
5.55 BTU-in/hr-ft²-°F
Silicone Property; ASTM E 1530
1.35 W/m-K
9.37 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM D1356
Electrical Properties Metric English Comments
Dielectric Strength 39.4 kV/mm
1000 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 141 °C
0.250 hour

@Temperature 285 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 4.44 - 10.0 °C
6.00 Month

@Temperature 40.0 - 50.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color White
Total Product Weight (g/m2) 325
Arlon SQA-TMS-025