Arlon UltraPad™ 51073G031D Silicone-Based Press Pad

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Ultrapad™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon UltraPad™ 51073G031D Silicone-Based Press Pad.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 211 microns
8.30 mil
Substrate; Arlon SQA-TMS-003
290 microns
11.4 mil
Side 1; Arlon SQA-TMS-003
290 microns
11.4 mil
Side 2; Arlon SQA-TMS-003
790 microns
31.1 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Silicone Property; ASTM D2240
81
81
Product Property; ASTM D2240
Tensile Strength 7.79 MPa
1130 psi
Silicone Property; ASTM D412
Elongation at Break 850 %
850 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 - 300 °C

@Pressure 0.000 - 5.00 MPa
302 - 572 °F

@Pressure 0.000 - 725 psi
Recommended Application Range
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 22.8 °C
60.0 Month

@Temperature 73.0 °F
Descriptive Properties Value Comments
Color Green
Product Property
Red
Substrate Property
Service Life 114 hours
at 225°C and 2.07 MPa
Total Product Weight (oz/yd2) 26.2
Arlon SQA-TMS-025