Armstrong A-4/E Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Armstrong Epoxy Adhesives; Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Armstrong A-4/E Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is a heavy, non-metallic filled, gray paste epoxy that provides excellent thixotropic non-sag bond lines. It can be used for small volume casting applications.Information provided by Ellsworth Adhesives.
Physical Properties Metric English Comments
Viscosity 500000 cP
500000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Tensile Strength, Ultimate 27.9 MPa
4050 psi
after optimum cure
Elongation at Break 2.7 %
2.7 %
Adhesive Bond Strength 56.9 MPa
8250 psi
Steel-Steel; after optimum cure
9.31 MPa

@Temperature 25.0 °C
1350 psi

@Temperature 77.0 °F
Aluminum-Aluminum tensile shear
16.5 MPa

@Temperature 82.2 °C
2400 psi

@Temperature 180 °F
Aluminum-Aluminum tensile shear
16.5 MPa

@Temperature -54.4 °C
2400 psi

@Temperature -66.0 °F
Aluminum-Aluminum tensile shear
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
Glass Transition Temp, Tg 101 °C
214 °F
Processing Properties Metric English Comments
Processing Temperature 93.3 °C
200 °F
Optimum cure is 1 hr. @ 200°F
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 g
Descriptive Properties Value Comments
Color Grey
Mix Ratio 100/6
By Weight