Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass F-Clean® Film for Greenhouses

Category Polymer , Film , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded
Manufacturer Asahi Glass Company
Trade Name F-Clean®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass F-Clean® Film for Greenhouses.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
F-CLEAN®, produced by Asahi Glass Company, Ltd., is a Ethylene-Tetrafluoroethylene copolymer (ETFE) film used as the preferred covering material for horticultural greenhouses. High tensile strength compared with other plastic films High visible light transmission exceeds 90% and provides an environment inside the greenhouse very similar to outdoors. Low degradation from sunlight and heat. Useful lifetime usually exceeds ten years. Very easily cleaned by rain and snow. Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 39.0 MPa
>= 5660 psi
JIS K7127
Elongation at Break 200 - 510 %
200 - 510 %
JIS K7127
Thermal Properties Metric English Comments
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 260 °C
500 °F
Maximum Service Temperature, Air 150 - 180 °C
302 - 356 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1e+6 Hz
2.6

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 120 kV/mm
3050 kV/in
ASTM D149
Dissipation Factor 0.00060

@Frequency 60 Hz
0.00060

@Frequency 60 Hz
ASTM D150
0.00080

@Frequency 1000 Hz
0.00080

@Frequency 1000 Hz
ASTM D150
0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz
ASTM D150
0.010

@Frequency 1e+9 Hz
0.010

@Frequency 1e+9 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Descriptive Properties Value Comments
Chemical Resistance Excellent
Copyright © lookpolymers.com All Rights Reserved