Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass Fluon® ETFE Film

Category Polymer , Film , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Fluorocarbon ETFE/ECTFE, Molded/Extruded
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® ETFE Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electronics, Energy Saving, Wallpaper, Sound Suppression Walls, Aviation and SpaceInformation provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.75 g/cc
1.75 g/cc
ASTM D792
Water Absorption 0.030 %
0.030 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 39.0 MPa
>= 5660 psi
JIS K7127
Elongation at Break 200 - 510 %
200 - 510 %
JIS K7127
Thermal Properties Metric English Comments
CTE, linear 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 260 °C
500 °F
Maximum Service Temperature, Air 150 - 180 °C
302 - 356 °F
Continuous
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.6

@Frequency 1e+6 Hz
2.6

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 120 kV/mm
3050 kV/in
ASTM D149
Dissipation Factor 0.00060

@Frequency 60 Hz
0.00060

@Frequency 60 Hz
ASTM D150
0.00080

@Frequency 1000 Hz
0.00080

@Frequency 1000 Hz
ASTM D150
0.0050

@Frequency 1e+6 Hz
0.0050

@Frequency 1e+6 Hz
ASTM D150
0.010

@Frequency 1e+9 Hz
0.010

@Frequency 1e+9 Hz
ASTM D150
Arc Resistance 120 sec
120 sec
ASTM D495
Descriptive Properties Value Comments
Chemical Resistance Excellent
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved