Asahi Glass Fluon® LM-740AP LM-ETFE Fluororesin

Category Polymer , Thermoplastic , Fluoropolymer , ETFE/ECTFE , Modified ETFE, Unreinforced
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® LM-740AP LM-ETFE Fluororesin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluon®LM-ETFE combines the excellent properties in heat resistance and other mechanical properties owned by ETFE resin and the low melting point.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Melt Flow 30 - 40 g/10 min
30 - 40 g/10 min
ASTM D359
Mechanical Properties Metric English Comments
Tensile Strength at Break 38.0 MPa
5510 psi
ASTM D638
Elongation at Break 420 %
420 %
ASTM D638
Descriptive Properties Value Comments
Heat Ageing (retention of elongation) 117%
Heat Ageing (retention of tensile strength) 88%