Asahi Kasei Lynex-T TFC64N Acetal Copolymer, Conductive Grade

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Asahi Kasei
Trade Name Lynex-T
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Lynex-T TFC64N Acetal Copolymer, Conductive Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acetal copolymer-based alloy with excellent electrical conductivity.Applications: Electroconductive parts.