Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P-40FG-0860 40% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 108 MPa
15700 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Flexural Strength 146 MPa
21200 psi
ASTM D790
Flexural Modulus 6.89 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.23 J/cm
2.30 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 32.4 µm/m-°C

@Temperature 20.0 °C
18.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
290 °F
ASTM D648