Asahi Kasei Thermylon® LSG-440A 60% Ceramic and Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Asahi Kasei
Trade Name Thermylon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylon® LSG-440A 60% Ceramic and Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.73 g/cc
1.73 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Strength 296 MPa
43000 psi
ASTM D790
Flexural Modulus 15.2 GPa
2200 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.7 J/cm
20.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 263 °C
505 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C
489 °F
ASTM D648
Flammability, UL94 HB
HB
0.0591 in thickness