Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 41 Nylon 66, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance and resistance to many chemicals, machine and motor oils, solvents and gasoline. Vydyne 41 is designed to meet the critical low-temperature impact requirements called out in many automotive specifications.Availability:Asia PacificEuropeNorth America Additive:Impact Modifier Features:Gasoline ResistanceGood Abrasion ResistanceGood Chemical ResistanceGood ProcessabilityHigh Impact ResistanceImpact ModifiedLow Temperature Impact ResistanceOil ResistantSolvent ResistantUses:AppliancesAutomotive ApplicationsConnectorsConsumer ApplicationsElectrical/Electronic ApplicationsFastenersGears Industrial ApplicationsAppearance: Natural ColorForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ISO 1183
Water Absorption 1.0 %
1.0 %
24 hrs; ISO 62
Moisture Absorption at Equilibrium 2.1 %
2.1 %
50% RH; ISO 62
Linear Mold Shrinkage 0.018 cm/cm

@Thickness 2.00 mm
0.018 in/in

@Thickness 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.016 cm/cm

@Thickness 2.00 mm
0.016 in/in

@Thickness 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 39.0 MPa
5660 psi
ISO 527-2
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO 527-2
Elongation at Break 180 %
180 %
ISO 527-2
Tensile Modulus 1.39 GPa
202 ksi
ISO 527-2
Flexural Strength 17.0 MPa
2470 psi
ISO 178
Flexural Modulus 0.545 GPa
79.0 ksi
ISO 178
Izod Impact, Notched (ISO) 25.0 kJ/m²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
ISO 180
29.0 kJ/m²

@Temperature -30.0 °C
13.8 ft-lb/in²

@Temperature -22.0 °F
ISO 180
88.0 kJ/m²

@Temperature 23.0 °C
41.9 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 2.50 J/cm²

@Temperature -40.0 °C
11.9 ft-lb/in²

@Temperature -40.0 °F
ISO 179
2.50 J/cm²

@Temperature -30.0 °C
11.9 ft-lb/in²

@Temperature -22.0 °F
ISO 179
11.0 J/cm²

@Temperature 23.0 °C
52.4 ft-lb/in²

@Temperature 73.4 °F
ISO 179