Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® 63A Nylon 66, General Purpose, medium viscosity, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® 63A Nylon 66, General Purpose, medium viscosity, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® 63A is a medium-viscosity resin used for injection-molding and extrusion-compounding. It is desirable to include this neat resin in a formulation in which the melt strength of the final product is critical for the application. Vydyne 63A exhibits good initial color and it has a moisture level below 0.1%. This product offers high strength, rigidity and toughness over a broad range of demanding applications. Resistance of Vydyne 63A to heat, oil and wear is typical of PA66 neat resins. Typical Applications/End Uses: Injection-molding, compounding, extrusion.Availability:Asia PacificEuropeNorth America Features:Gasoline ResistanceGeneral PurposeGood Chemical ResistanceGood Color StabilityOil ResistantSolvent ResistantUses:CompoundingGeneral PurposeAppearance: Natural ColorForms: PelletsProcessing Method: Compounding and Compounding ExtrusionInformation provided by Ascend
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Bulk Density 0.674 g/cc
0.0243 lb/in³
ASTM D1895
Relative Viscosity 75 - 90 cP
75 - 90 cP
ASTM D789
Viscosity Measurement 183 - 200
183 - 200
[cm3/g], H2SO4 (Sulphuric Acid); ISO 307
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 3146
Optical Properties Metric English Comments
Yellow Index 2.0 %
2.0 %
ASTM D1925
Processing Properties Metric English Comments
Moisture Content 0.10 %
0.10 %
ASTM D6869
Copyright © lookpolymers.com All Rights Reserved