Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced, Flame Retardant
Manufacturer Ascend Performance Materials (formerly Solutia)
Trade Name VYDYNE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machine feed and easy mold release and has Underwriters Laboratories UL 94 flammability classification of V-0 at 0.4 mm (0.016”) thick.Availability:Asia PacificEuropeNorth America Additive:Flame RetardantLubricant Features:DuctileFlame RetardantGood Crack ResistanceGood Mold ReleaseGood ToughnessHalogen Free Low DensityLubricatedUses:AppliancesAutomotive ElectronicsBobbinsConnectorsElectrical HousingElectrical PartsElectrical/Electronic ApplicationsFastenersIndustrial ApplicationsLighting ApplicationsLiving HingesPrinted Circuit BoardsSwitchesAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation provided by Ascend Performance Materials.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Water Absorption 0.80 %

@Time 86400 sec
0.80 %

@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Diameter 2.00 mm
0.0090 in/in

@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm

@Diameter 2.00 mm
0.0060 in/in

@Diameter 0.0787 in
ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.00 MPa
580 psi
ISO 527-2
Tensile Strength, Yield 83.0 MPa
12000 psi
ISO 527-2
Flexural Strength 107 MPa
15500 psi
ISO 178
Flexural Modulus 3.90 GPa
566 ksi
ISO 178
Poissons Ratio 0.40
0.40
ISO 527-2
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180
Charpy Impact Unnotched 7.50 J/cm²

@Temperature 23.0 °C
35.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
7.80 J/cm²

@Temperature -30.0 °C
37.1 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.340 J/cm²

@Temperature 23.0 °C
1.62 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
0.370 J/cm²

@Temperature -30.0 °C
1.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 265 °C
509 °F
ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 240 °C
464 °F
Unannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Unannealed; ISO 75-2/A
UL RTI, Electrical 120 °C

@Thickness 0.400 mm
248 °F

@Thickness 0.0157 in
UL 746
120 °C

@Thickness 0.750 mm
248 °F

@Thickness 0.0295 in
UL 746
120 °C

@Thickness 1.50 mm
248 °F

@Thickness 0.0591 in
UL 746
120 °C

@Thickness 3.00 mm
248 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical with Impact 75.0 °C

@Thickness 0.400 mm
167 °F

@Thickness 0.0157 in
UL 746
80.0 °C

@Thickness 0.750 mm
176 °F

@Thickness 0.0295 in
UL 746
80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
80.0 °C

@Thickness 3.00 mm
176 °F

@Thickness 0.118 in
UL 746
UL RTI, Mechanical without Impact 105 °C

@Thickness 0.400 mm
221 °F

@Thickness 0.0157 in
UL 746
110 °C

@Thickness 0.750 mm
230 °F

@Thickness 0.0295 in
UL 746
110 °C

@Thickness 1.50 mm
230 °F

@Thickness 0.0591 in
UL 746
110 °C

@Thickness 3.00 mm
230 °F

@Thickness 0.118 in
UL 746
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Glow Wire Test 700 °C

@Thickness 1.50 mm
1290 °F

@Thickness 0.0591 in
Ignition Temperature; IEC 60695-2-13
700 °C

@Thickness 3.00 mm
1290 °F

@Thickness 0.118 in
Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 0.400 mm
1760 °F

@Thickness 0.0157 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 1.50 mm
1760 °F

@Thickness 0.0591 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
Flammability Index; IEC 60695-2-12
960 °C

@Thickness 0.400 mm
1760 °F

@Thickness 0.0157 in
Ignition Temperature; IEC 60695-2-13
960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
Ignition Temperature; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm

@Thickness 0.750 mm
1.00e+10 ohm-cm

@Thickness 0.0295 in
IEC 60093
Dielectric Strength 17.0 kV/mm

@Thickness 1.00 mm
432 kV/in

@Thickness 0.0394 in
IEC 60243
Arc Resistance 120 - 179 sec

@Thickness 3.00 mm
120 - 179 sec

@Thickness 0.118 in
ASTM D495
Comparative Tracking Index 600 V

@Thickness 3.00 mm
600 V

@Thickness 0.118 in
IEC 60112
Hot Wire Ignition, HWI 7.0 - 14 sec

@Thickness 0.400 mm
7.0 - 14 sec

@Thickness 0.0157 in
UL 746
7.0 - 14 sec

@Thickness 0.750 mm
7.0 - 14 sec

@Thickness 0.0295 in
UL 746
15 - 29 sec

@Thickness 1.50 mm
15 - 29 sec

@Thickness 0.0591 in
UL 746
30 - 59 sec

@Thickness 3.00 mm
30 - 59 sec

@Thickness 0.118 in
UL 746
High Amp Arc Ignition, HAI 30 - 59 arcs

@Thickness 0.400 mm
30 - 59 arcs

@Thickness 0.0157 in
UL 746
60 - 119 arcs

@Thickness 0.750 mm
60 - 119 arcs

@Thickness 0.0295 in
UL 746
60 - 119 arcs

@Thickness 1.50 mm
60 - 119 arcs

@Thickness 0.0591 in
UL 746
60 - 119 arcs

@Thickness 3.00 mm
60 - 119 arcs

@Thickness 0.118 in
UL 746
High Voltage Arc-Tracking Rate, HVTR 0.000 - 10.0 mm/min
0.000 - 0.394 in/min
UL 746
Processing Properties Metric English Comments
Rear Barrel Temperature 260 - 290 °C
500 - 554 °F
Middle Barrel Temperature 260 - 290 °C
500 - 554 °F
Front Barrel Temperature 260 - 290 °C
500 - 554 °F
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Melt Temperature 270 - 285 °C
518 - 545 °F
Mold Temperature 65.0 - 95.0 °C
149 - 203 °F
Drying Temperature 80.0 °C
176 °F
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved