Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 20% Glass Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 265 PPO, 20% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A general purpose, 20% glass reinforced PPO resin for injection molding applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 82.0 MPa
11900 psi
ATSM D638
Elongation at Break 4.3 %
4.3 %
ASTM D638
Flexural Modulus 4.90 GPa
711 ksi
ASTM D790
Izod Impact, Notched 0.920 J/cm
1.72 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 134 °C
273 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
ASTM D648