Ashley Polymers Ashlene® 531 Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 531 Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
For Monofilament spinning/super dry.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ASTM D792
Apparent Bulk Density 0.700 g/cc
0.0253 lb/in³
ASTM D1895
Thermal Properties Metric English Comments
Melting Point 258 °C
496 °F
ASTM D3418