Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 742L-33G Nylon 6/66, 33% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
6/66 Copolymer with high surface gloss in addition to high stiffness and strength, 33% Glass Reinforced.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ASTM D792
Water Absorption 1.8 %
1.8 %
ASTM D570
Water Absorption at Saturation 6.5 %
6.5 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 162 MPa
23500 psi
ASTM D638
Elongation at Break 4.5 %
4.5 %
Flexural Modulus 6.90 GPa
1000 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 200 °C
392 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
351 °F
ASTM D648
Users viewing this material also viewed the following: