Ashley Polymers Ashlene® 990L-30G Nylon 610, 30% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 990L-30G Nylon 610, 30% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% glass reinforced for excellent dimensional stability and low water absorption.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.20 %
0.20 %
ASTM D570
Linear Mold Shrinkage 0.0035 cm/cm
0.0035 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 131 MPa
19000 psi
ATSM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 200 MPa
29000 psi
ASTM D790
Flexural Modulus 6.60 GPa
957 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 216 °C
421 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 460 ohm-cm
460 ohm-cm
ASTM D257