Material Notes:
Medium impact, low flow, rigid with a matte finish. Suitable for injection molding and also extrusion for thin walls like refrigerator liners.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Melt Flow 0.42 g/10 min
0.42 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Izod Impact, Notched 1.34 J/cm
2.51 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.950 J/cm²

@Thickness 6.00 mm
4.52 ft-lb/in²

@Thickness 0.236 in
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 98.0 °C
208 °F
ASTM D648
Vicat Softening Point 108 °C
226 °F
ASTM D1525