Material Notes:
General purpose super high impact with good gloss.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Melt Flow 0.40 g/10 min
0.40 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Ultimate 138 MPa
20000 psi
ATSM D638
Flexural Strength 57.0 MPa
8270 psi
ASTM D790
Flexural Modulus 1.90 GPa
276 ksi
ASTM D790
Izod Impact, Notched 3.92 J/cm
7.34 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
ASTM D648
Flammability, UL94 HB
HB