Material Notes:
A general purpose V-2 and V-0 rated resin for injection molding.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ATSM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.0 °C
199 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
UL94