Material Notes:
General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
High Load Melt Index 6.5 g/10 min

@Load 21.6 kg,
Temperature 260 °C
6.5 g/10 min

@Load 47.6 lb,
Temperature 500 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ATSM D638
Elongation at Break 77 %
77 %
ASTM D638
Flexural Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Izod Impact, Notched 5.66 J/cm
10.6 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ASTM D648