Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Asia Technology Pioneers
Trade Name CAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asia Technology Pioneers CAN 102 Acrylic Hi-Compound Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ACN 102 is hi-tech compounded Acrylic Resin. This hi-composite is produced by Nano-Technology and used widely in paint and Coating industryAdvantages:High abrasion and corrosion resistanceHigh UV resistanceHigh scratch resistanceOutstanding surface appearanceCertification:ISO 9001:2008Iranian Nano Technology Initiative Council CertificationApplication:Traffic Marking PaintInformation provided by Asia Technology Pioneers
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
ASTM D1475
Solids Content 60 %
60 %
ASTM 1259
Viscosity 15000 - 25000 cP
15000 - 25000 cP
ASTM D562
Mechanical Properties Metric English Comments
Abrasion 0.023
0.023
[Gr], 33% improvement; ASTM D4060
Chemical Properties Metric English Comments
Acid Value <= 10
<= 10
Descriptive Properties Value Comments
Impedance Analyses Water uptake ~ 10
Salt Spray Resistance High Improved
ASTM 117
Solvent Toluene
Thermal behaviors High Improved