Material Notes:
AA-BOND 2103 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting and improved mechanical electrical properties is required. AA-BOND 2103 is two-part liquid epoxy adhesive contains no solvents and is easy to mix, use and apply at room temperature. AA-BOND 2103 develops strong, rigid, high performance bonds to itself and to ceramics, glass and glass fabrics, metals, laminates and other composite materials, forestry and masonry products, and to most rigid plastics. AA-BOND 2103 is an effective electrical insulator, and further provides excellent resistance to weather, galvanic action, vapors, JP4 fuel, gasoline, lubricants and other petroleum products, mild acids and alkalis, salts, and other organic and inorganic compounds.Appearance: Clear, slight hazeCure Type: Heat cure or Room TemperatureBenefits:Good wettingGreat mechanical propertiesGreat electrical propertiesSolvent freeEasy mix and apply Mix Ratio by weight: 100:25/Resin:HardenerSubstrates: Ceramics, glass to glass, fabrics, metals, laminates and other composite materialsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Izod Impact, Notched 0.107 J/cm
0.200 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 52.0 µm/m-°C
28.9 µin/in-°F
Maximum Service Temperature, Air 125 °C
257 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
Dielectric Constant 4.1

@Frequency 420 Hz
4.1

@Frequency 420 Hz
Dissipation Factor 0.020
0.020
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 20.0 min
20.0 min