Atom Adhesives AA-BOND 2156 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND 2156 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND 2156 is a thixotropic (smooth paste) thermally conductive epoxy system. It is used for staking heat sinks, transistors, diodes, resistor, integrated circuits and other heat-sensitive components to printed circuit boards. AA-BOND 2156 is two parts fast cure adhesive develops strong bond to many materials, and its coefficient of thermal expansion provides a good match for the application.Appearance: TanCure Type: Heat cure or Room TemperatureBenefits:Fast CureStrongDurableHigh impact bonds at room temperature that improves heat Mix Ratio by weight: 100:23/Resin:Hardener Substrates: Bonds readily to itself and to metals, silica, steatite, alumina, sapphire and other ceramics, glass, plastics and to many other materials Typical Application: Fiber optic bundles, potting glass fibers and fiber optic connectorsInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.294 g/cc
2.294 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Viscosity 11000 - 13000 cP
11000 - 13000 cP
Uncured, after Mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
Shear Strength 23.4 MPa
3400 psi
Lap, Alum to Alum
Adhesive Bond Strength 23.4 MPa
3400 psi
Thermal Properties Metric English Comments
CTE, linear 25.9 µm/m-°C
14.4 µin/in-°F
Thermal Conductivity 0.840 W/m-K
5.83 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 33.0 °C
91.4 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 33.0 °C
91.4 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 25.0 °C
1.00 hour

@Temperature 77.0 °F
180 min

@Temperature 65.0 °C
3.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 5.00 min
5.00 min
uncured
Shelf Life 12.0 Month
12.0 Month