Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Atom Adhesives AA-BOND FDA16 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND FDA16 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval.Appearance: Amber Cure Type: Heat cure or Room TemperatureBenefits:Medium viscosityClass VI approvedLow permeabilityGood resistance Mix Ratio by weight: 100:33/Resin:Hardener Typical Application: Bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
cured
Solids Content 100 %
100 %
uncured
Volatile Organic Compounds (VOC) Content 0.15 g/l
0.15 g/l
uncured
Water Absorption at Saturation 0.30 %

@Time 86400 sec
0.30 %

@Time 24.0 hour
uncured
Viscosity 4700 cP
4700 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 75

@Temperature 25.0 °C,
Time 86400 sec
75

@Temperature 77.0 °F,
Time 24.0 hour
86

@Temperature 65.0 °C,
Time 14400 sec
86

@Temperature 149 °F,
Time 4.00 hour
Shear Strength 14.5 MPa

@Temperature 25.0 °C,
Time 86400 sec
2100 psi

@Temperature 77.0 °F,
Time 24.0 hour
Lap, Alum to Alum
22.8 MPa

@Temperature 65.0 °C,
Time 14400 sec
3300 psi

@Temperature 149 °F,
Time 4.00 hour
Lap, Alum to Alum
Thermal Properties Metric English Comments
CTE, linear 52.9 µm/m-°C
29.4 µin/in-°F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 97.0 °C
207 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Copyright © lookpolymers.com All Rights Reserved