Axiall 14890 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 14890 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose UL approved 720 hour sunlight resistant jacket suitable for a maximum 80°C temperature rating at a 1/32" wall. Recommended for UF-B and NM-B constructions and also RG59 coaxial cable jackets.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 - 1.42 g/cc
1.38 - 1.42 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 86 - 92
86 - 92
delayed; ASTM D-2240
Tensile Strength, Yield 18.10 MPa
2625 psi
ASTM D-638
Elongation at Yield 275.6 %
275.6 %
Air Aging: 168 hours @ 113°C; 30 mil slabs; UL 1581
325 %
325 %
ASTM D-638
100% Modulus 0.01155 GPa
1.675 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D-746
Oxygen Index 24 %
24 %
ASTM D-638
Processing Properties Metric English Comments
Melt Temperature 188 °C
370 °F