Axiall 19940-03 Wire & Cable Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 19940-03 Wire & Cable Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
THHN-THWN circuit sizes. Best suited for 1/64 wall, 18 AWG and smaller. UL recognized for THHN, THW, THWN, TW. Oil resistant II and VW-1 rated.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 - 1.39 g/cc
1.35 - 1.39 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore A 91 - 97
91 - 97
delayed; ASTM D-2240
Hardness, Shore D 42 - 48
42 - 48
delayed; ASTM D-2240
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D-638
Elongation at Yield 291.5 %
291.5 %
Air Aging: 168 hours @ 136°C; UL 1581
293.2 %
293.2 %
Oil Aging: 4 hours @ 70°C; #2 Oil; 30 mil slabs; UL 1581
325 %
325 %
ASTM D-638
100% Modulus 0.0148 GPa
2.15 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -18.0 °C
-0.400 °F
ASTM D-746
Oxygen Index 30 %
30 %
ASTM D-638
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
50% RH; ASTM D-257
Processing Properties Metric English Comments
Melt Temperature 193 °C
380 °F