Axiall 2512 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 2512 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D-638
Elongation at Yield 2.6 %
2.6 %
ASTM D-638
Tensile Modulus 3.28 GPa
475 ksi
ASTM D-638
Izod Impact, Notched 1.17 J/cm

@Thickness 6.35 mm
2.20 ft-lb/in

@Thickness 0.250 in
ASTM D-256
1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 95.5 kJ/m²
45.5 ft-lb/in²
ASTM D-1822