Material Notes:
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 85
85
ASTM D-785
Tensile Strength, Yield 43.4 MPa
6300 psi
ASTM D-638
Tensile Modulus 2.74 GPa
398 ksi
ASTM D-638
Flexural Strength 73.22 MPa
10620 psi
ASTM D-790
Flexural Modulus 2.55 GPa
370 ksi
ASTM D-790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
1.50 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
5.34 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
10.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 22.0 J

@Temperature 23.0 °C
16.2 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 67 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.72 °C
164.7 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.72 °C
159.3 °F
ASTM D-648
UL RTI, Electrical 95.0 °C
203 °F
UL-746B
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL-746B
UL RTI, Mechanical without Impact 95.0 °C
203 °F
UL-746B
Flammability, UL94 5VA
5VA
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390°F) 190
Internal